SIFAT FISIK DAN MEKANIK PAPAN PARTIKEL AKIBAT PENAMBAHAN FILLER SERAT BAMBU

Physical and Mechanical Properties of Particle Board Due to Addition of Filler Bamboo Fibre

Authors

Aryani Rofaida , Rizki Mikroji Pratama , I Wayan Sugiartha , Desi Widianty

DOI:

10.29303/spektrum.v8i1.187

Published:

2021-03-20

Issue:

Vol. 8 No. 1 (2021): SPEKTRUM SIPIL

Keywords:

Papan Partikel, Filler serat bambu, Sifat Fisik, Sifat Mekanik

Articles

Downloads

How to Cite

Rofaida, A., Pratama, R. M., Sugiartha, I. W., & Widianty, D. (2021). SIFAT FISIK DAN MEKANIK PAPAN PARTIKEL AKIBAT PENAMBAHAN FILLER SERAT BAMBU: Physical and Mechanical Properties of Particle Board Due to Addition of Filler Bamboo Fibre. Spektrum Sipil, 8(1), 1–11. https://doi.org/10.29303/spektrum.v8i1.187

Downloads

Download data is not yet available.

Metrics

Metrics Loading ...

Abstract

Bambu adalah salah satu sumber daya alam yang mudah diperoleh dan diperbaharui, sehingga menjadi alternatif pengganti untuk pembuatan papan partikel kayu. Studi ini mengelaborasi sifat fisik maupun mekanik papan partikel kayu yang diperoleh secara eksperimen kemudian dibandingkan dengan ketentuan yang terdapat dalam Standar SNI 03-2105-2006. Ukuran papan partikel yang akan diuji sesuai dengan standar SNI 03-2105-2006, Pengujian yang dilakukan yaitu pengujian sifat fisik dan mekanik meliputi : uji kerapatan, kadar air, daya serap air, pengembangan tebal setelah direndam air, Modulus of Rupture (MOR), Modulus of Elasticity (MOE), keteguhan rekat, dan keteguhan cabut sekrup.Tujuannya adalah untuk mengetahui perilaku fisik dan mekanik papan partikel akibat adanya penambahan filler serat bambu. Hasil pengujian pengembangan tebal papan partikel menunjukkan bahwa pengembangan tebal papan partikel dengan penambahan filler serat bambu  mempunyai nilai pengembangan tebal terendah yaitu 4,504 %. Berdasarkan standar SNI 03-2015-2006 nilai pengembangan tebal yaitu ≤ 12 %. Sedangkan nilai sifat mekanik dengan rata-rata nilai MOR adalah 95.395 MPa, nilai MOE adalah 68,7996 MPa,nilai keteguhan rekat adalah 48,38 MPa, dan uji kuat tarik sekrup 1105,25 N.

Author Biographies

Aryani Rofaida, Universitass Mataram

Rizki Mikroji Pratama, Universitas Mataram

I Wayan Sugiartha, Universitas Mataram

Desi Widianty, Universitas Mataram

License

Copyright (c) 2021 Aryani Rofaida, Rizki Mikroji Pratama, I Wayan Sugiartha, Desi Widianty

Creative Commons License

This work is licensed under a Creative Commons Attribution 4.0 International License.

You are free to:

  • Share — copy and redistribute the material in any medium or format for any purpose, even commercially.
  • Adapt — remix, transform, and build upon the material for any purpose, even commercially.

The licensor cannot revoke these freedoms as long as you follow the license terms.

Under the following terms:

  • Attribution — You must give appropriate credit, provide a link to the license, and indicate if changes were made. You may do so in any reasonable manner, but not in any way that suggests the licensor endorses you or your use.
  • No additional restrictions — You may not apply legal terms or technological measures that legally restrict others from doing anything the license permits.

Notices:

You do not have to comply with the license for elements of the material in the public domain or where your use is permitted by an applicable exception or limitation.

No warranties are given. The license may not give you all of the permissions necessary for your intended use. For example, other rights such as publicity, privacy, or moral rights may limit how you use the material.

Most read articles by the same author(s)

<< < 1 2 3 4 > >> 

Similar Articles

1 2 3 4 5 6 > >> 

You may also start an advanced similarity search for this article.