KUAT TEKAN DAN KUAT GESER BAMBU KOMPOSIT SETEMPAT BERPENGISI PLASTIK DAN SERBUK GERGAJI KAYU

Compressive Strength and Shear Strength of Local Composite Bamboo Filled Plastic and Wood Sawdust

Authors

I Wayan Sugiartha , Aryani Rofaida , Teti Handayani , Rini S Saptaningtyas

DOI:

10.29303/spektrum.v8i1.194

Published:

2021-03-20

Issue:

Vol. 8 No. 1 (2021): SPEKTRUM SIPIL

Keywords:

bambu, kuat tekan, kuat geser, plastik, PET, sserbuk gergaji kayu

Articles

Downloads

How to Cite

Sugiartha, I. W., Rofaida, A., Handayani, T., & Saptaningtyas, R. S. (2021). KUAT TEKAN DAN KUAT GESER BAMBU KOMPOSIT SETEMPAT BERPENGISI PLASTIK DAN SERBUK GERGAJI KAYU: Compressive Strength and Shear Strength of Local Composite Bamboo Filled Plastic and Wood Sawdust. Spektrum Sipil, 8(1), 27–31. https://doi.org/10.29303/spektrum.v8i1.194

Downloads

Download data is not yet available.

Metrics

Metrics Loading ...

Abstract

Bambu merupakan salah satu alternatif bahan bangunan ramah lingkungan,yang dapat menggantikan kayu. Disamping memiliki banyak keunggulan, bambu juga memiliki kelemahan yaitu kuat geser sejajar seratnya rendah. Solusi untuk mengatasi kelemahan tersebut adalah dengan memberikan bahan pengisi pada ruas bambu disekitar sambungan sehingga terjadi komposit setempat. Penelitian ini bertujuan untuk mengetahui sifat mekanik (kuat tekan dan kuat geser) bambu komposit setempat berpengisi plastik Polyethylane Terephthalate (PET) dan serbuk gergaji kayu. Lima variasi benda uji dibuat yaitu BK-0 (bambu tanpa pengisi sebagai kontrol), BK-1 (bambu berpengisi plastik PET), BK-2 (bambu berpengisi plastik PET + dilabur perekat), BK-3 (bambu berpengisi plastik PET + serbuk gergaji kayu), BK-4 (bambu berpengisi plastik PET + serbuk gergaji kayu dan dilabur perekat). Hasil pengujian memberikan nilai kuat tekan  bambu dari  BK-0 sampai dengan BK-4 berturut-turut sebesar 22.7 MPa, 29.4 MPa, 32.7 MPa, 33.2 MPa, 35.7 MPa atau terjadi peningkatan kuat tekan terhadap  BK-0 berturut-turut sebesar 30%, 44%, 46%, dan 57%.  Sedangkan nilai kuat geser bambu dari BK-0 sampai dengan BK-4 berturut-turut sebesar  4.55 MPa, 5.00 MPa, 5.05 MPa, 5.40 MPa, 5.50 MPa atau terjadi peningkatan kuat geser terhadap  BK-0 berturut-turut sebesar 10%, 11%, 19%, dan 21%.

Author Biographies

I Wayan Sugiartha, Universitas Mataram

Aryani Rofaida, Universitas Mataram

Teti Handayani, Universitas Mataram

Rini S Saptaningtyas, Universitas Mataram

License

Copyright (c) 2021 I Wayan Sugiartha, Aryani Rofaida, Teti Handayani, Rini S Saptaningtyas

Creative Commons License

This work is licensed under a Creative Commons Attribution 4.0 International License.

You are free to:

  • Share — copy and redistribute the material in any medium or format for any purpose, even commercially.
  • Adapt — remix, transform, and build upon the material for any purpose, even commercially.

The licensor cannot revoke these freedoms as long as you follow the license terms.

Under the following terms:

  • Attribution — You must give appropriate credit, provide a link to the license, and indicate if changes were made. You may do so in any reasonable manner, but not in any way that suggests the licensor endorses you or your use.
  • No additional restrictions — You may not apply legal terms or technological measures that legally restrict others from doing anything the license permits.

Notices:

You do not have to comply with the license for elements of the material in the public domain or where your use is permitted by an applicable exception or limitation.

No warranties are given. The license may not give you all of the permissions necessary for your intended use. For example, other rights such as publicity, privacy, or moral rights may limit how you use the material.

Most read articles by the same author(s)

1 2 > >>